Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Kalrez® 6221 FFKM Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Kalrez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Kalrez® 6221 FFKM Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Kalrez® parts made from compounds 6221 provide superior chemical resistance and low contamination from extractables in pharmaceutical and food handling applications where FDA compliance is required. Compounds 6221 and 6230 are especially suited for Water For Injection (WFI) systems, Steam in-Place (SIP) cleaning and other critical systems.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 75
65 - 75
Tensile Strength, Ultimate 15.17 MPa
2200 psi
500 mm/min; ASTM D412
Elongation at Break 150 %
150 %
500 mm/min; ASTM D412
100% Modulus 0.00724 GPa
1.05 ksi
Compression Set 20 %

@Temperature 160 °C
20 %

@Temperature 320 °F
70 hr; ASTM D395B, Size 214 O-rings
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Descriptive Properties Value Comments
Color White