DuPont Performance Polymers Zytel® HTN LT51G35HSLR BL661A Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Zytel® HTN
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont Performance Polymers Zytel® HTN LT51G35HSLR BL661A Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
35% Glass Reinforced Laser Weldable PPA High Performance Polyamide Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 235 MPa
34100 psi
DAM; ISO 527-1/-2
Elongation at Break 2.4 %
2.4 %
DAM; ISO 527-1/-2
Tensile Modulus 11.8 GPa
1710 ksi
DAM; ISO 527-1/-2
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 262 °C
504 °F
DAM; ISO 75-1/-2
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Processing Injection Moulding
Regional Availability Asia Pacific
Special Characteristics Heat stabilised or stable to heat