DuPont Teijin Films Melinex® 461 Polyester Film

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 461 Polyester Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Melinex® 461 is a high clarity polyester film manufactured with a coating on one surface that promotes adhesion to many solvent formulations and to most vinyl or acrylic base ink systems. The adhesion pretreated surface is wound outside of the roll.Typical Applications: Melinex 461 is used in many general industrial applications where clarity and adhesion properties are critical, e.g., coating, lamination and label applications.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD >= 89.6 MPa
>= 13000 psi
ASTM D882A
Film Tensile Strength at Yield, TD >= 89.6 MPa
>= 13000 psi
ASTM D882A
Coefficient of Friction, Dynamic <= 0.70
<= 0.70
A-B; ASTM D1894
Film Tensile Strength at Break, MD >= 172 MPa
>= 25000 psi
ASTM D882A
Film Tensile Strength at Break, TD >= 172 MPa
>= 25000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 13969 in2/lb
for 142 Gauge