Eagle Brass 194 HSM® Copper, 1/2 Hard

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Eagle Brass Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 194 HSM® Copper, 1/2 Hard.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and plateability. Applications include connectors, semiconductor pins and leadframes, sockets and mass terminations.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.91 g/cc
0.322 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 52 - 63
52 - 63
Thickness > 0.020 Inch
Tensile Strength, Ultimate 365 - 434 MPa
53000 - 63000 psi
Tensile Strength, Yield 248 - 421 MPa
36000 - 61000 psi
0.2% offset
Elongation at Break 6.0 - 29 %
6.0 - 29 %
in 2 in.
Tensile Modulus 121 GPa
17500 ksi
Thermal Properties Metric English Comments
CTE, linear 17.6 µm/m-°C

@Temperature 20.0 - 300 °C
9.80 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 259 W/m-K
1800 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 97.5 %
97.5 %
Iron, Fe 2.35 %
2.35 %
Phosphorous, P 0.030 %
0.030 %
Zinc, Zn 0.12 %
0.12 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000198 ohm-cm
0.00000198 ohm-cm
Annealed