Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eagle Brass 230 Red Brass, 1/2 Hard

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Eagle Brass Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 230 Red Brass, 1/2 Hard.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, fasteners, conduit, heat exchangers, flexible metal hose, pipe, and couplings.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.75 g/cc
0.316 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 56 - 64
56 - 64
Thickness > 0.020 Inch
Tensile Strength, Ultimate 352 - 421 MPa
51000 - 61000 psi
Tensile Strength, Yield 296 - 372 MPa
43000 - 54000 psi
0.2% offset
Elongation at Break 8.0 - 21 %
8.0 - 21 %
in 2 in.
Tensile Modulus 117 GPa
17000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.7 µm/m-°C

@Temperature 20.0 - 300 °C
10.4 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 159.1 W/m-K
1104 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 85 %
85 %
Zinc, Zn 15 %
15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000481 ohm-cm
0.00000481 ohm-cm