Material Notes:
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.86 g/cc
0.320 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 74 - 78
74 - 78
Thickness > 0.020 Inch
Tensile Strength, Ultimate 607 - 710 MPa
88000 - 103000 psi
Tensile Strength, Yield 586 - 703 MPa
85000 - 102000 psi
0.2% offset
Elongation at Break 2.0 - 6.0 %
2.0 - 6.0 %
in 2 in.
Tensile Modulus 110 GPa
16000 ksi
Thermal Properties Metric English Comments
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 69.2 W/m-K
480 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 94.9 %
94.9 %
Phosphorous, P 0.10 %
0.10 %
Tin, Sn 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001187 ohm-cm
0.00001187 ohm-cm
Annealed