Eagle Brass 752 Nickel Silver 18%, Annealed

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Eagle Brass Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 752 Nickel Silver 18%, Annealed.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.75 g/cc
0.316 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 39 - 60
39 - 60
Thickness > 0.020 Inch
Tensile Strength, Ultimate 365 - 434 MPa
53000 - 63000 psi
Tensile Strength, Yield 124 - 221 MPa
18000 - 32000 psi
0.2% offset
Elongation at Break 29 - 42 %
29 - 42 %
in 2 in.
Tensile Modulus 124 GPa
18000 ksi
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 32.9 W/m-K
228 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 65 %
65 %
Nickel, Ni 18 %
18 %
Zinc, Zn 17 %
17 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000297 ohm-cm
0.0000297 ohm-cm