Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 8.00 g/cc
8.00 g/cc
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
ISO 527
Elongation at Break 525 %
525 %
ISO 527
Flexural Modulus 0.180 GPa
26.1 ksi
ISO 178
Izod Impact, Notched NB
NB
ISO 180-A
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F
Drying Temperature 70.0 °C
158 °F
Dry Time 2 - 4 hour
2 - 4 hour