Elastocon TPE Technologies Elastocon® SMR1555 Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® SMR1555 Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Elastocon® SMR1555 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. Elastocon® SMR1555 is well suited for consumer goods and industrial applications requiring U.V. stability and excellent low temperature stability. Elastocon® SMR1555 provides a non-bloom surface.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ASTM D2240
Tensile Strength, Yield 16.8 MPa
2440 psi
ASTM D412
Elongation at Break 583 %
583 %
ASTM D412
100% Modulus 0.0136 GPa
1.97 ksi
ASTM D412
Dynatup @ -30°C 38.6 J
28.5 ft-lb
ASTM D3763
Processing Properties Metric English Comments
Rear Barrel Temperature 200 - 225 °C
392 - 437 °F
Front Barrel Temperature 200 - 230 °C
392 - 446 °F
Nozzle Temperature 200 - 235 °C
392 - 455 °F
Mold Temperature 21.0 - 49.0 °C
69.8 - 120 °F
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
Descriptive Properties Value Comments
Injection Velocity (mm/sec) Fast