Ensinger Tecapeek® XP-93 Compression Molded PEEK Compound, 30% PTFE Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, PTFE-Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-93 Compression Molded PEEK Compound, 30% PTFE Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Filler Content 30 %
30 %
Mechanical Properties Metric English Comments
Tensile Strength 51.7 MPa
7500 psi
ASTM D638
Elongation at Break 3.8 %
3.8 %
ASTM D638
4.0 %
4.0 %
Flexural Strain; ASTM D790
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Izod Impact, Notched 0.278 J/cm
0.520 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Descriptive Properties Value Comments
Color Tan