Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength 1.2 mil Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength 1.2 mil Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior properties along with the resin's good drawdown capability permit usage in many demanding packaging applicationsApplications: Merchandise bags; Frozen food packaging; Heavy duty bags; Sandwich bags; Liners. Data for film properties below based on 1.2 mil film.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
Exxon Method
Thickness 30.5 microns
1.20 mil
Melt Flow 1.3 g/10 min
1.3 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.6 MPa
1540 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.9 MPa
1730 psi
ASTM D882
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Film Elongation at Break, TD 730 %
730 %
ASTM D882
Secant Modulus, MD 0.254 GPa
36.8 ksi
ASTM D882
Secant Modulus, TD 0.261 GPa
37.9 ksi
ASTM D882
Elmendorf Tear Strength MD 290 g
290 g
ASTM D1922
Elmendorf Tear Strength TD 650 g
650 g
ASTM D1922
Elmendorf Tear Strength, MD 9.53 g/micron
242 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 21.3 g/micron
542 g/mil
ASTM D1922
Dart Drop 5.24 g/micron
133 g/mil
F50; ASTM D1709
Dart Drop Test 160 g
0.353 lb
F50; ASTM D-1709
Film Tensile Strength at Break, MD 51.6 MPa
7480 psi
ASTM D882
Film Tensile Strength at Break, TD 42.2 MPa
6120 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
Exxon Method
Optical Properties Metric English Comments
Haze 25 %
25 %
ASTM D1003
Gloss 27 %
27 %
45°, ASTM D-2457