ExxonMobil Exxtral™ CNU 017 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ CNU 017 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by high flow, high stiffness, low odor and emissions that is typically used automotive air conditioning units.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/ToughnessGood Impact ResistanceGood Surface FinishLow EmissionsLow to No Odor Uses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.911 g/cc
0.0329 lb/in³
ISO 1183
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.0 MPa
2610 psi
ISO 527-2/50
Tensile Strength, Yield 31.0 MPa
4500 psi
ISO 527-2/50
Elongation at Break 35 %
35 %
ISO 527-2/50
Elongation at Yield 4.4 %
4.4 %
ISO 527-2/50
Tensile Modulus 1.75 GPa
254 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.357 J/cm²

@Temperature 0.000 °C
1.70 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
0.567 J/cm²

@Temperature 22.8 °C
2.70 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 53.9 °C
129 °F
ISO 75-2/A