Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LDPE LD 358BW Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 358BW Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: LD 358BW is an EVA LDPE which offers a combination of excellent sealability and toughness even at low temperatures.Availability: Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: YesApplications: Agricultural FilmCo-Extrusion FilmsConstruction FilmFoamsForm Fill and Seal PackagingFreezer FilmHeavy Duty BagsIce BagsProfile ExtrusionInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ExxonMobil method
Vinyl Acetate Content 4.0 %
4.0 %
ExxonMobil Method
Melt Flow 0.28 g/10 min
0.28 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 500 %
500 %
ASTM D882
Film Elongation at Break, TD 650 %
650 %
ASTM D882
Elmendorf Tear Strength MD 220 g
220 g
ASTM D1922
Elmendorf Tear Strength TD 350 g
350 g
ASTM D1922
Dart Drop Test 640 g
1.41 lb
ASTM D1709A
Film Tensile Strength at Break, MD 29.0 MPa
4200 psi
ASTM D882
Film Tensile Strength at Break, TD 26.9 MPa
3900 psi
ASTM D882
1% Secant Modulus, MD 152 MPa
22000 psi
ASTM D882
1% Secant Modulus, TD 159 MPa
23000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 221 °C
<= 430 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 9.1 %
9.1 %
ASTM D1003