Fainplast Compounds PG 56/B Flexible PVC, Extrusion Modified with Rubber

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds PG 56/B Flexible PVC, Extrusion Modified with Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hydrocarbon resisting tubes
Physical Properties Metric English Comments
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 53 - 57
53 - 57
ISO R 868
Tensile Strength at Break 13.0 MPa
1890 psi
ISO R 527
Elongation at Break 360 %
360 %
ISO R 527