Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

FloMet 7% Ni/Fe Low Alloy Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer FloMet LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF FloMet 7% Ni/Fe Low Alloy Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume metal powder and 40% volume plastic. The mixture (referred to as feedstock) is then injection molded at relatively low temperatures and pressures in conventional plastic injection molding machines. The molded green parts are then thermally processed in two steps. First, the binder is removed by evaporation in an operation called debinding. Next, the part is sintered in a dry hydrogen atmosphere, which densifies the part isotropically. The complex shape of the original molded part is retained throughout the process, and close tolerances can be achieved. Density is typically 95-98% of the wrought metal; mechanical properties and corrosion resistance are similar to wrought materialInformation provided by FloMet LLC.
Mechanical Properties Metric English Comments
Hardness, Rockwell B 70
70
Tensile Strength, Ultimate 400 MPa
58000 psi
Tensile Strength, Yield 283 MPa

@Strain 0.200 %
41000 psi

@Strain 0.200 %
Elongation at Break 32 %
32 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Iron, Fe 93 %
93 %
As remainder
Nickel, Ni 7.0 %
7.0 %
Users viewing this material also viewed the following: