Global PP-1126-NK Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Global Polymers Corporation
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Global PP-1126-NK Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description-transparency, high stiffness, high heat resistantApplications- food applicationsInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
L; ASTM D1238
Mechanical Properties Metric English Comments
Ball Indentation Hardness 85.0 MPa
12300 psi
DIN 53456
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Shear Modulus 0.700 GPa
102 ksi
DIN 53457
Charpy Impact, Notched 0.280 J/cm²

@Temperature -23.0 °C
1.33 ft-lb/in²

@Temperature -9.40 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Unannealed; ASTM D648