Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global ST-1018 Low Density Polyethylene, Injection Molding Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Global ST-1018 Low Density Polyethylene, Injection Molding Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 for use in direct contact with foodInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.03 MPa
1020 psi
ASTM D638
Tensile Strength, Yield 9.03 MPa
1310 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 82.8 °C
181 °F
ASTM D1525