Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1200 °C
2190 °F
Component Elements Properties Metric English Comments
Nickel, Ni 70 %
70 %
Titanium, Ti 30 %
30 %