Haveg Havaflex T.A.-118 Phenolic, Trowelable Ablative Coating

Category Polymer , Thermoset , Phenolic , Phenolic, Ablative Coating
Manufacturer Haveg
Trade Name Havaflex
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haveg Havaflex T.A.-118 Phenolic, Trowelable Ablative Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A two-component modified phenolic ablative coating and adhesive. This material was developed for the U.S. Army to protect the areas around missile launching systems from the extremely high heats (up to 5000°F) and gas velocities (up to Mach 3.0) present during the launching of a missile.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Moisture Absorption at Equilibrium 0.67 %
0.67 %
96 Hours
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
Tensile Strength, Ultimate 4.30 MPa
624 psi
Elongation at Break 12.5 %
12.5 %
Adhesive Bond Strength 23.0 MPa
3340 psi
Tensile Lap Shear; ASTM D1002
Thermal Properties Metric English Comments
Thermal Conductivity 0.513 W/m-K
3.56 BTU-in/hr-ft²-°F