Hexcel® HexForce™ 104 Fiber Glass Fabric

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Hexcel
Trade Name HexForce™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexForce™ 104 Fiber Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential allowing the end user to choose the best combination for material performance, economics and product flexibility.Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 27.9 microns
1.10 mil
Mechanical Properties Metric English Comments
Tensile Impact 10.7 J/cm
20.0 ft-lb/in
Filling Breaking Strength
32.0 J/cm
60.0 ft-lb/in
Warp Breaking Strength
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 0.57
Dry
Nominal Construction (count/in) 52
Fill
60
Warp
Type of Yarn Fill Yarn: ECD 1800 1/0
Warp Yarn: ECD 900 1/0
Weave Style Plain