| Category | Polymer , Thermoset , Epoxy , Epoxy Cure Resin |
| Manufacturer | Hexcel |
| Trade Name | HexPly® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/48370/1000.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.28 g/cc | 0.0462 lb/in³ | Resin |
| 1.53 g/cc | 0.0553 lb/in³ | Nominal Laminate | |
| 1.78 g/cc | 0.0643 lb/in³ | Fibre |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 1022 MPa @Temperature 23.0 °C |
148200 psi @Temperature 73.4 °F |
prEN2561 Type B |
| Tensile Modulus | 58.0 GPa @Temperature 23.0 °C |
8410 ksi @Temperature 73.4 °F |
prEN2561 Type B |
| Compressive Yield Strength | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
Compression After Impact @ 6.7 J/mm; AITM 1.0010 |
| 765 MPa @Temperature 23.0 °C |
111000 psi @Temperature 73.4 °F |
prEN2580 Type B | |
| Compressive Modulus | 50.0 GPa @Temperature 23.0 °C |
7250 ksi @Temperature 73.4 °F |
prEN2580 Type B |
| Shear Modulus | 4.60 GPa @Temperature 23.0 °C |
667 ksi @Temperature 73.4 °F |
In-Plane; prEN6032 |
| Shear Strength | 48.4 MPa @Temperature 23.0 °C |
7020 psi @Temperature 73.4 °F |
ILSS; prEN2563 |
| 77.0 MPa @Temperature 23.0 °C |
11200 psi @Temperature 73.4 °F |
In-Plane; prEN6032 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | 201 °C | 394 °F | Onset |
| 218 °C | 424 °F | Peak |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Shelf Life | 12.0 Month @Temperature -18.0 °C |
12.0 Month @Temperature -0.400 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Cured Thickness per Ply (cm) | 0.0417 | |
| Fiber Volume (%) | 49.8 | |
| Tack Life (days) | 15 |