| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Shelf Life | 12.0 Month | 12.0 Month | Normal Storing Conditions |
|
Premix Thermoplastics PRE-ELEC® PE 1271
PRE-ELEC PE 1271 is a conductive thermoplastic compound based on a blend of PE-LD/PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivi..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | Normal Storing Conditions |
|
Premix Thermoplastics PRE-ELEC® PE 1292
PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | Liquid State |
|
Palm Labs Adhesives Turbo Fuse Series 110 (5 Viscosity) Rapid Bonding Adhesive
Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
|
|||
| Shelf Life |
12.0
Month @Temperature -17.8 °C |
12.0
Month @Temperature 0.000 °F |
|
|
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, T-700 24K Uni-Tape Reinforced
Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
Permabond ES578 Epoxy Resin
PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bon..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
Permabond TA4300 Toughened Acrylic Adhesive
PERMABOND® TA4300 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue...
|
|||
| Shelf Life |
12.0
Month @Temperature 20.0 - 30.0 °C |
12.0
Month @Temperature 68.0 - 86.0 °F |
|
|
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
Permabond MM115P Pure Anaerobic Threadlocker
Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
Michelman® Licomer® W 19 Anionic / Nonionic polyethylene emulsion
Description: Anionic / Nonionic polyethylene emulsionUsage: Licomer® W 19 is an emulsion designed for floor polish formulations providing high hardness and gloss. This emulsion forms a clear film..
|
|||
| Shelf Life |
12.0
Month @Temperature 21.0 - 27.0 °C |
12.0
Month @Temperature 69.8 - 80.6 °F |
|
|
Lord Adhesives HPC-6B Ethylene Acrylic Elastomer Coating
LORD HPC-6B and HPC-6C are one-part, room temperature curing ethylene acrylic elastomer (AEM) coatings which feature robust adhesion and exceptional mechanical properties. These coatings enhance ozo..
|
|||
| Shelf Life |
12.0
Month @Temperature -40.0 °C |
12.0
Month @Temperature -40.0 °F |
|
|
Tra-Con Tra-Bond 77-2LTC Low Temperature Cure SMD Adhesive
TRA-BOND 77-2LTC one component, solvent-free, insulative epoxy adhesive is designed to cure at temperatures as low as 80°C. This adhesive is specifically designed for attaching surface mounted devi..
|
|||
| Shelf Life |
12.0
Month @Temperature 23.9 °C |
12.0
Month @Temperature 75.0 °F |
in unopened container |
|
Master Bond EP30ND Non-Drip, Dimensionally Stable Epoxy Adhesive
Description: Master Bond Polymer System EP30ND is a high viscosity, two component epoxy adhesive/sealant with a paste consistency. It will cure at room temperature or more rapidly at elevated temper..
|
|||
| Shelf Life |
12.0
Month @Temperature -40.0 °C |
12.0
Month @Temperature -40.0 °F |
|
|
Tra-Con Tra-Bond 9070D Filled Epoxy Adhesive
TRA-BOND 9070D filled epoxy adhesive exhibits a low coefficient of expansion. Information provided by Tra-Con Inc.
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
Dow Corning SLYGARD® 527 A&B SILICONE DIELECTRIC GEL
Two-parts, clear, RT or heat cure.Information provided by Dow Corning
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
Dow Corning SYL-OFF® 7210 RELEASE MODIFIER
Syl-Off® 7210 Release Modifier is a 60% active solids, pre-catalysed, release modifier. General purpose release modifier recommeded for use with Syl-Off® Solvent based, platinum catalysed release ..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
Dow Corning SYL-OFF® 7677 RELEASE COATING
Syl-Off® 7677 Coating is a 100% active solids pre-catalysed, coating containing a medium viscosity hexenyl endblocked only functional silicone polymer. Recommended for use against aggressive adhesi..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | Shelf Life Time at 25°C in original, unopened containers. |
|
Cytec Conathane® CC-1194 (Conap) Polyurethane Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
|
|||
| Shelf Life |
12.0
Month @Temperature 25.0 °C |
12.0
Month @Temperature 77.0 °F |
|
|
Epoxy Technology EPO-TEK® 310M-T Flexible Epoxy
Material Description: A two component, flexible epoxy designed for low stress applications in semiconductor, hybrid, medical, acoustical and optical industries. Replacement for EPO-TEK® 310T.Info..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
Dow Corning 3715 TOPCOAT
A 2 part solventless silicone top coat that cures to a very hard and very low friction surface that is anti-soiling and dirt repellent. It is suitable as a top coat on high friction, blocking silico..
|
|||
| Shelf Life |
12.0
Month @Temperature 23.9 °C |
12.0
Month @Temperature 75.0 °F |
From date of manufacture |
|
Arlon 51582R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Inform..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
3M 9738R Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
|
|||
| Shelf Life |
12.0
Month @Temperature 21.1 °C |
12.0
Month @Temperature 70.0 °F |
|
|
Arlon 920-10CxxFR-P1 0.020" Self-Fusing Silicone Rubber Tape
1 inch wide, 20 mil thick, brown, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De..
|
|||
| Shelf Life |
12.0
Month @Temperature 23.9 °C |
12.0
Month @Temperature 75.0 °F |
From date of manufacture |
|
Arlon HS930-10R##-P4 0.030" (0.762 mm) Self-Fusing Silicone Tape (Rectangular, Unsupported)
Description: High Strength, 1 inch wide, 30 mil thick, Red, Rectangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicat..
|
|||
| Shelf Life |
12.0
Month @Temperature 23.9 °C |
12.0
Month @Temperature 75.0 °F |
From date of manufacture |
|
Arlon LW401R##-P0 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i..
|
|||
| Shelf Life |
12.0
Month @Temperature 21.1 °C |
12.0
Month @Temperature 70.0 °F |
From date of manufacture |
|
Arlon R35782R010 0.0105" (0.267 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 FiberglassThis data represents typical values for the production mat..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
3M Scotchkote™ 2400 Pipe Renewal Liner
NSF/ANSI-61 certified polyurea formulation is 100% solids and contains no epoxy resin. It is designed to help solve a wide variety of problems common to potable water systems. It utilizes a trenchle..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | |
|
3M 7220SA Screen Printable Polyester Performance Label Products with Structured Adhesive
3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc..
|
|||
| Shelf Life | 12.0 Month | 12.0 Month | in unopened containers |
|
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System
Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to..
|
|||