Download PDF Hexcel® HexWeb® CR-PAA™ 1/8-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the face sheets that carry bending loads and the honeycomb that carries the shear loads. The adhesive is the interface between the facing and the core in the same way that the oxide on the aluminum and the primer that has been applied to it is the interface between the honeycomb substrate material and the bonding adhesive. This interface is critical to the performance of honeycomb bonded assemblies.HexWeb® CR-PAA™ is designed for aircraft structures that are exposed to demanding environmental conditions. HexWeb® CR-PAA™ outperforms standard MIL-C-7438 core in salt spray and HexWeb® crack propagation tests.
Physical Properties Metric English Comments
Density 0.0977 g/cc
0.00353 lb/in³
Nominal
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 5.24 MPa
>= 760 psi
Bare, min
>= 5.69 MPa
>= 825 psi
Stabilized, min
7.72 MPa
1120 psi
Bare, typ
8.27 MPa
1200 psi
Stabilized, typ
Compressive Modulus 2.03 GPa
295 ksi
Stabilized, typ
Shear Modulus 0.262 GPa
38.0 ksi
Plate Shear, W Direction, typ
0.703 GPa
102 ksi
Plate Shear, L Direction, typ
Shear Strength >= 2.10 MPa
>= 305 psi
Plate Shear, W Direction, min
2.76 MPa
400 psi
Plate Shear, W Direction, typ
>= 3.62 MPa
>= 525 psi
Plate Shear, L Direction, min
4.76 MPa
690 psi
Plate Shear, L Direction, typ