Material Notes:
Weight per Epoxide (EEW, g/eq) 2300 to 2800. Max color is 2.Comments/Applications: Unmodified bis A "Type 9" epoxy. Lower molecular weight GT 6610 US. High melt viscosity epoxy for high quality industrial coatings and container coatings.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 145 - 155 °C
293 - 311 °F
Softening Range