Material Notes:
Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, multi-layer systems, and personal care films.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)3.2.aFilm properties based on 0.95 guage (24 µm) thickness; blow-up ratio 2:1.Information provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505
Thickness 24.1 microns
0.950 mil
Melt Flow 4.4 g/10 min
4.4 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.290 GPa
42.1 ksi
ASTM D882
Secant Modulus, TD 0.340 GPa
49.3 ksi
ASTM D882
Elmendorf Tear Strength MD 40 g
40 g
ASTM D1922
Elmendorf Tear Strength TD 450 g
450 g
ASTM D1922
Elmendorf Tear Strength, MD 1.65 g/micron
42.0 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 18.7 g/micron
474 g/mil
ASTM D1922
Dart Drop 2.09 g/micron
53.0 g/mil
ASTM D1709
Dart Drop Test 50.0 g
0.110 lb
ASTM D1709
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ASTM D882
Film Tensile Strength at Break, TD 18.0 MPa
2610 psi
ASTM D882
Optical Properties Metric English Comments
Haze 2.1 %
2.1 %
ASTM D1003
Gloss 90 %
90 %
at 45°; ASTM D523
Processing Properties Metric English Comments
Melt Temperature 260 - 290 °C
500 - 554 °F