| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
PolyOne Bergamid™ A70 G35 H U BK SO Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
PolyOne Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)
These products contain flame retardants which are activated by longer residence times in the cylinder and then can decompose. At interruption of the moulding cycle (approx. >5 min) it is recommended..
|
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
|
PolyOne Edgetek® XT XT-100-CX01 PC+PBT
(discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
|
|||
| Melt Temperature | 260 - 277 °C | 500 - 530 °F | Molding |
|
PolyOne Therma-Tech™ NJ-6000C TC Nylon 12
(discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
|
|||
| Melt Temperature | 260 - 300 °C | 500 - 572 °F | Average value: 283 °C Grade Count:14 |
|
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
|
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
|
|||
| Melt Temperature | 260 °C | 500 °F | for test specimens; ISO 294 |
|
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Melt Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS.
|
|||
| Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
|
Lanxess Pocan® B 3215 Z 000000 PBT, 10% Glass Fiber
PBT, 10% glass fibers, injection molding, impact modified
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber
PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS.
|
|||
| Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
|
Lanxess Pocan® BF 4409 000000 PBT, 7% Glass Fiber
PBT, 7% glass fibers, injection molding, flame retardant
|
|||
| Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
|
Lanxess Pocan® C 3230 XF 000000 PBT + PC, 30% Glass Fiber
PBT+PC, 30% glass fibers, injection molding, improved flowability, low tendency to warp, improved surface finish
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Styron EMERGEâ„¢ 8600-20 Polycarbonate
EMERGEâ„¢ PC 8600-20 is a translucent, ignition-resistant and easy flow polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global ..
|
|||
| Melt Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Tisan TISLAMID® 66 30% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melt Temperature | 260 - 320 °C | 500 - 608 °F | Die Melt Temp |
|
Total LDPE LA 0710 Low Density Polyethylene - Extrusion Coating
LDPE LA 0710 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum. High draw down, low neck in.In..
|
|||
| Melt Temperature | 260 °C | 500 °F | Injection molding; ISO 294 |
|
Covestro Bayblend® FR3050 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
|
|||
| Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
|
Covestro Bayblend® T65 Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 120 °Cgood low temperature impact strengthPreprocessingMax. Water content
|
|||
| Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
|
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch..
|
|||
| Melt Temperature | 260 - 290 °C | 500 - 554 °F | |
|
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
|
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
|
|||
| Melt Temperature | 260 °C | 500 °F | for shrinkage test |
|
BASF Ultradur B 2550 PBT
Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in..
|
|||
| Melt Temperature | 260 °C | 500 °F | for shrinkage test |
|
BASF Ultradur B 4300 G4 20% Glass Filled PBT
Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
|
|||
| Melt Temperature | 260 °C | 500 °F | for shrinkage test, Optimal |
|
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT
Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit..
|
|||
| Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
|
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | DAM |
|
DuPont Performance Polymers Zytel® 73G30TGI BK267 Nylon 6
(Unverified Data**)
Zytel® 73G30TGI BK267 is a 30% glass fiber reinforced, toughened, black polyamide 6 optimized for gas injection molding process.Information provided by DuPont Performance Polymers
|
|||
| Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
|
Lanxess Pocan® S 7020 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
|
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose
Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical
|
|||