I. Stern IS-35955 High Density Polyethylene, Blow Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer I. Stern & Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF I. Stern IS-35955 High Density Polyethylene, Blow Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features:IS-35955 is designed for applications requiring excellent stiffness and stress crack resistance properties.Meets all requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contactApplicationsGeneral purpose blow molding and sheet extrusionInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D1238
Environmental Stress Crack Resistance 35 hour
35 hour
Condition B; ASTM D1693
45 hour
45 hour
Condition A; ASTM D1693
Melt Flow 0.35 g/10 min
0.35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D638
Elongation at Yield 600 %
600 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= 82.2 °C
<= 180 °F
ASTM D746