| Category | Ceramic , Oxide , Aluminum Oxide |
| Manufacturer | International Ceramic Engineering |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | ICE Al2O3 96.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.96 g/cc | 0.143 lb/in³ | |
| Water Absorption | 0.00 % | 0.00 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Mohs | 9.0 | 9.0 | |
| Tensile Strength, Ultimate | 170 MPa | 24700 psi | |
| Flexural Strength | 310 MPa | 45000 psi | |
| Compressive Strength | 2590 MPa | 376000 psi | |
| Fracture Toughness | 4.50 MPa-m½ | 4.10 ksi-in½ |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 7.50 µm/m-°C @Temperature 25.0 - 600 °C |
4.17 µin/in-°F @Temperature 77.0 - 1110 °F |
|
| Thermal Conductivity | 24.7 W/m-K | 171 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 1750 °C | 3180 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 96 % | 96 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 9.3 @Frequency 1e+6 Hz |
9.3 @Frequency 1e+6 Hz |
|
| Dielectric Strength | 9.10 kV/mm | 231 kV/in | |
| Dielectric Loss Index | 0.0028 | 0.0028 | 1 MHz, 25°C (77°F) |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | White |