| Category | Polymer , Adhesive , Thermoset |
| Manufacturer | ITW Devcon |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | ITW Devcon Metal Repair Bronze Putty (BR), Bronze.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.23 g/cc | 0.0806 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 85 | 85 | Cured; ASTM D2240 |
| Tensile Strength at Break | 18.2 MPa | 2640 psi | ASTM D638 |
| Modulus of Elasticity | 5.52 GPa | 800 ksi | ASTM D638 |
| Flexural Strength | 42.6 MPa | 6180 psi | ASTM D790 |
| Compressive Strength | 58.9 MPa | 8540 psi | ASTM D695 |
| Adhesive Bond Strength | 18.5 MPa | 2680 psi | tensile shear; ASTM D1002 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Thermal Conductivity | 0.657 W/m-K | 4.55 BTU-in/hr-ft²-°F | ASTM C177 |
| Maximum Service Temperature, Air | 121 °C | 250 °F | dry |
| Shrinkage | 0.10 % | 0.10 % | Cured; ASTM D2566 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 75 @Frequency 1000 Hz |
75 @Frequency 1000 Hz |
ASTM D150 |
| Dielectric Strength | 0.984 kV/mm | 25.0 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 960 min | 16.0 hour | Functional cure |
| Pot Life | 35.0 min @Temperature 23.9 °C |
35.0 min @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Coverage per pound, in² @ 1/4" thickness | 50 | |
| Mix ratio by volume (Resin:Hardener) | 3:1 | |
| Mix ratio by weight (Resin:Hardener) | 9:1 |