| Category | Polymer , Adhesive , Thermoset |
| Manufacturer | ITW Devcon |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | ITW Devcon Metal Repair Titanium Putty, Grey.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.37 g/cc | 0.0855 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 87 | 87 | Cured; ASTM D2240 |
| Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
| Modulus of Elasticity | 6.55 GPa | 950 ksi | ASTM D638 |
| Flexural Strength | 53.1 MPa | 7700 psi | ASTM D790 |
| Compressive Strength | 130 MPa | 18800 psi | ASTM D695 |
| Adhesive Bond Strength | 13.8 MPa | 2000 psi | tensile shear; ASTM D1002 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 39.6 µm/m-°C @Temperature 20.0 °C |
22.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Thermal Conductivity | 0.816 W/m-K | 5.65 BTU-in/hr-ft²-°F | ASTM C177 |
| Maximum Service Temperature, Air | 177 °C | 350 °F | dry |
| Shrinkage | 0.10 % | 0.10 % | Cured; ASTM D2566 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 44.8 @Frequency 1000 Hz |
44.8 @Frequency 1000 Hz |
ASTM D150 |
| Dielectric Strength | 2.20 kV/mm | 56.0 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 960 min | 16.0 hour | Functional cure |
| Pot Life | 21.0 min @Temperature 23.9 °C |
21.0 min @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Coverage per pound, in² @ 1/4" thickness | 47 | |
| Mix ratio by volume (Resin:Hardener) | 3:1 | |
| Mix ratio by weight (Resin:Hardener) | 4.3:1 |