| Category | Polymer , Adhesive , Thermoset , Polyurethane, TS |
| Manufacturer | ITW Devcon |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | ITW Devcon Rubber Repair / Castable Urethane Edge & Seal (T-35), Black.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0377 lb/in³ | |
| Viscosity | 5000 cP | 5000 cP | Mixed Viscosity |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 94 | 94 | Cured; ASTM D2240 |
| Tensile Strength at Break | 22.8 MPa | 3300 psi | ASTM D412 |
| Elongation at Break | <= 450 % | <= 450 % | ASTM D412 |
| Tear Strength | 75.4 kN/m | 430 pli | ASTM D624 |
| Taber Abrasion, mg/1000 Cycles | 250 | 250 | H-18 wheel (1000 gram load) |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
| 82.2 °C | 180 °F | dry | |
| Shrinkage | 0.14 % | 0.14 % | Cured; ASTM D2566 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 90.0 min | 1.50 hour | Functional cure |
| Pot Life | 3.00 min @Temperature 23.9 °C |
3.00 min @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Coverage per pound, in² @ 1/4" thickness | 106 | |
| Mix ratio by weight (Resin:Hardener) | 80:20 |