Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy 168 Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 168 Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 11.19 g/cc
0.4043 lb/in³
Thermal Properties Metric English Comments
Melting Point 300 - 320 °C
572 - 608 °F
Solidus 300 °C
572 °F
Liquidus 320 °C
608 °F
Component Elements Properties Metric English Comments
Antimony, Sb 2.0 %
2.0 %
Lead, Pb 98 %
98 %