Indium Corp. Indalloy 195 Gold Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 195 Gold Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 15.67 g/cc
0.5661 lb/in³
Thermal Properties Metric English Comments
Melting Point 890 °C
1630 °F
Eutectic
Solidus 890 °C
1630 °F
Liquidus 890 °C
1630 °F
Component Elements Properties Metric English Comments
Copper, Cu 20 %
20 %
Gold, Au 80 %
80 %