Indium Corp. Indalloy 197 Bismuth Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 197 Bismuth Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 10.25 g/cc
0.3703 lb/in³
Thermal Properties Metric English Comments
Melting Point 92.0 °C
198 °F
Eutectic
Solidus 92.0 °C
198 °F
Liquidus 92.0 °C
198 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 51.6 %
51.6 %
Cadmium, Cd 8.2 %
8.2 %
Lead, Pb 40.2 %
40.2 %