| Category | Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy |
| Manufacturer | Indium Corporation of America |
| Trade Name | Indalloy |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Indium Corp. Indalloy 217-440 Bismuth-Lead-Tin Solder Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 9.30 g/cc | 0.336 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Brinell | 19 | 19 | |
| Tensile Strength at Break | 89.6 MPa | 13000 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 0.167 J/g-°C | 0.0399 BTU/lb-°F | Solid |
| Melting Point | 103 - 227 °C | 217 - 441 °F | |
| Solidus | 103 °C | 217 °F | |
| Liquidus | 227 °C | 441 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Antimony, Sb | 9.0 % | 9.0 % | |
| Bismuth, Bi | 48 % | 48 % | |
| Lead, Pb | 28.5 % | 28.5 % | |
| Tin, Sn | 14.5 % | 14.5 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000570 ohm-cm | 0.0000570 ohm-cm |