Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy® 255 Bi-Pb Fusible Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 255 Bi-Pb Fusible Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose fusible alloy. Poor solderability.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 10.44 g/cc
0.3772 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 15
15
Tensile Strength, Ultimate 44.1 MPa
6400 psi
Elongation at Break 37.5 %
37.5 %
Thermal Properties Metric English Comments
Heat of Fusion 20.9 J/g
8.99 BTU/lb
Specific Heat Capacity 0.126 J/g-°C
0.0301 BTU/lb-°F
Solid
0.155 J/g-°C
0.0370 BTU/lb-°F
Liquid
Thermal Conductivity 4.00 W/m-K

@Temperature 85.0 °C
27.8 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 124 °C
255 °F
Eutectic
Solidus 124 °C
255 °F
Liquidus 124 °C
255 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 55.5 %
55.5 %
Lead, Pb 44.5 %
44.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000430 ohm-cm
0.0000430 ohm-cm