Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , T 600 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name URANUS®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) to increase its structure stability and corrosion resistance. Due to combined additions of chromium (20%), molybdenum (4.3%), copper (1.5%) combined with its high nickel content, the grade is recommended for most applications dealing with medium to severe corrosive solutions. UR B6 has improved stress corrosion resistance properties. UR B6 alloy is particularly used in sulphuric and phosphoric acids applications. The localized corrosion resistance of UR B6N grade is much higher than that of alloy 825. UR B6N is particularly well adapted to clad plates applications (separators).Information provided by manufacturer.
Physical Properties Metric English Comments
Density 8.05 g/cc
0.291 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 160 - 210
160 - 210
Typical, V<sub>10</sub>
Tensile Strength, Ultimate >= 550 MPa
>= 79800 psi
Minimum Guaranteed
Tensile Strength, Yield >= 245 MPa
<br>@Strain 0.200 %
>= 35500 psi
<br>@Strain 0.200 %
>= 275 MPa
<br>@Strain 1.00 %
>= 39900 psi
<br>@Strain 1.00 %
Elongation at Break >= 40 %
>= 40 %
Modulus of Elasticity 200 GPa
29000 ksi
Poissons Ratio 0.333
0.333
Calculated
Shear Modulus 75.0 GPa
<br>@Temperature 20.0 °C
10900 ksi
<br>@Temperature 68.0 °F
Charpy Impact >= 100 J
<br>@Temperature -196 °C
>= 73.8 ft-lb
<br>@Temperature -321 °F
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C
<br>@Temperature 20.0 - 100 °C
8.33 µin/in-°F
<br>@Temperature 68.0 - 212 °F
16.0 µm/m-°C
<br>@Temperature 20.0 - 300 °C
8.89 µin/in-°F
<br>@Temperature 68.0 - 572 °F
17.0 µm/m-°C
<br>@Temperature 20.0 - 500 °C
9.44 µin/in-°F
<br>@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.500 J/g-°C
<br>@Temperature 20.0 °C
0.120 BTU/lb-°F
<br>@Temperature 68.0 °F
Thermal Conductivity 17.0 W/m-K
<br>@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F
<br>@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 20 %
20 %
Copper, Cu 1.5 %
1.5 %
Iron, Fe 49.18 %
49.18 %
As remainder
Molybdenum, Mo 4.3 %
4.3 %
Nickel, Ni 25 %
25 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000800 ohm-cm
<br>@Temperature 20.0 °C
0.0000800 ohm-cm
<br>@Temperature 68.0 °F