| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity |           1.60 - 1.70           g/cc           @Thickness 1.57 mm  | 
                  1.60 - 1.70           g/cc           @Thickness 0.0620 in  | 
        ASTM D792 | 
| Moisture Absorption at Equilibrium |           0.10 %                     @Thickness 1.57 mm  | 
                  0.10 %                     @Thickness 0.0620 in  | 
        ASTM D229 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Rockwell M |           95 - 115                     @Thickness 1.57 mm  | 
                  95 - 115                     @Thickness 0.0620 in  | 
        ASTM D785 | 
| Tensile Strength, Yield |           490           MPa           @Thickness 1.57 mm  | 
                  71000           psi           @Thickness 0.0620 in  | 
        CW; ASTM D638 | 
|           496           MPa           @Thickness 1.57 mm  | 
                  72000           psi           @Thickness 0.0620 in  | 
        LW; ASTM D638 | |
| Modulus of Elasticity |           36.5           GPa           @Thickness 1.57 mm  | 
                  5300           ksi           @Thickness 0.0620 in  | 
        CW; ASTM D229 | 
|           41.4           GPa           @Thickness 1.57 mm  | 
                  6000           ksi           @Thickness 0.0620 in  | 
        LW; ASTM D229 | |
| Flexural Strength |           676           MPa           @Thickness 1.57 mm  | 
                  98000           psi           @Thickness 0.0620 in  | 
        CW; ASTM D790 | 
|           679           MPa           @Thickness 1.57 mm  | 
                  98500           psi           @Thickness 0.0620 in  | 
        LW; ASTM D790 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear |           4.00           µm/m-°C           @Thickness 1.57 mm, Temperature 20.0 °C  | 
                  2.22           µin/in-°F           @Thickness 0.0620 in, Temperature 68.0 °F  | 
        x-axis; IPC-TM 650-2.4.24 | 
| CTE, linear, Transverse to Flow |           8.00           µm/m-°C           @Thickness 1.57 mm, Temperature 20.0 °C  | 
                  4.44           µin/in-°F           @Thickness 0.0620 in, Temperature 68.0 °F  | 
        x-axis; IPC-TM 650-2.4.24 | 
| Maximum Service Temperature, Air | 177 °C | 351 °F | |
| Glass Transition Temp, Tg | 125 °C | 257 °F | Tg | 
| Flammability, UL94 |           HB                     @Thickness 1.57 mm  | 