Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM 792
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
10 seconds; ASTM D2240
Tensile Strength, Yield 7.58 MPa
1100 psi
Elastic; ASTM D412
Elongation at Break 600 %
600 %
Elastic; ASTM D412
Flexural Modulus 0.112 GPa
16.3 ksi
ASTM D790
Tear Strength 42.1 kN/m
240 pli
ASTM D624