Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos R12C-01 Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos R12C-01 Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Grade R12C-01 is a high clarity, antistatic polypropylene copolymer for injection molding and stretch blow molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsConsumer products Housewares Medical Rigid packagingBenefitsUltra high clarity Excellent processability Good impact resistance at room and refrigerator temperatures Low taste and odor Excellent static control Microwavable
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790B
Izod Impact, Notched 1.01 J/cm

@Diameter 3.17 mm
1.90 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Optical Properties Metric English Comments
Haze 11 %

@Thickness 1.27 mm
11 %

@Thickness 0.0500 in
plaque; ASTM D1003
Descriptive Properties Value Comments
Process Blow Molding
Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: