| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | Iran Petrochemical Commercial Co. (PCC) |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Iran Petrochemical (PCC) PC 3038 Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D792 |
| Melt Flow | 30.1 - 38 g/10 min @Load 1.20 kg, Temperature 300 °C |
30.1 - 38 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | >= 103 MPa | >= 14900 psi | DIN 53456 |
| Tensile Stress | 55.0 - 70.0 MPa | 7980 - 10200 psi | ASTM D638 |
| Tensile Strength, Yield | >= 60.0 MPa | >= 8700 psi | ASTM D638 |
| Elongation at Break | >= 50 % | >= 50 % | ASTM D638 |
| Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 140 - 150 °C | 284 - 302 °F | 50 N, 50°C/h; ASTM D1525 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | >= 80 % @Thickness 2.00 mm |
>= 80 % @Thickness 0.0787 in |
ASTM D1003 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 2.8 - 3.1 @Frequency 1.00e+6 Hz |
2.8 - 3.1 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | >= 20.0 kV/mm @Frequency 50.0 Hz |
>= 508 kV/in @Frequency 50.0 Hz |
ASTM D149 |
| Dielectric Loss Index | 0.00080 - 0.0010 @Frequency 5.00e+7 Hz |
0.00080 - 0.0010 @Frequency 5.00e+7 Hz |
ASTM D150 |
| 0.0080 - 0.011 @Frequency 1.00e+6 Hz |
0.0080 - 0.011 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Solvent Content, ppm | < 500 | GC |