Isoflon PTFE + 15% Ceramic Polytetrafluoroethylene with 15% Ceramic

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Mica Filled
Manufacturer Isoflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PTFE + 15% Ceramic Polytetrafluoroethylene with 15% Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Properties:Improved compression resistanceGood dielectric characteristicsGood thermal insulationMachining can be trickyApplications: Electrical applicationsInformation provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 2.24 - 2.27 g/cc
2.24 - 2.27 g/cc
ASTM D792
Deformation 5.0 - 7.0 %

@Time 86400 sec
5.0 - 7.0 %

@Time 24.0 hour
Permanent, after Relaxation; ASTM D695
10 - 12 %

@Pressure 0.0000140 MPa,
Time 86400 sec
10 - 12 %

@Pressure 0.00203 psi,
Time 24.0 hour
Under Load; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 62 - 67
62 - 67
ASTM D2240
Tensile Strength 18.0 - 23.0 MPa
2610 - 3340 psi
ASTM D4894
Elongation at Break 200 - 250 %
200 - 250 %
ASTM D4894
Coefficient of Friction, Dynamic 0.28 - 0.30
0.28 - 0.30
ASTM D1894
Coefficient of Friction, Static 0.30 - 0.32
0.30 - 0.32
ASTM D1894
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Strength 20.0 - 25.0 kV/mm
508 - 635 kV/in
ASTM D149