Karina E 856-08/435-Y-ERYB Beige PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 856-08/435-Y-ERYB Beige PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Rigid PVC compound recommended for extrusion of profiles developed for Window City under L1555IVORY sample.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application General Purpose Profiles