Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kinlead ML11 General Grade BOPP Matt Film (thickness: 15 µm)

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Kinlead
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kinlead ML11 General Grade BOPP Matt Film (thickness: 15 µm).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ML11 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. One side has corona treatment. It is specially designed for board lamination with a matt finish on one side.Information provided by Kinlead.
Physical Properties Metric English Comments
Thickness 15.0 microns
0.591 mil
± 3.5%; ASTM-252-78
Linear Mold Shrinkage 0.040 cm/cm
0.040 in/in
ASTM-D1204
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ASTM-D1204
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 170 %
170 %
ASTM-D882
Film Elongation at Break, TD 65 %
65 %
ASTM-D882
Coefficient of Friction 0.30
0.30
T/T-US; ASTM-D1894
0.60
0.60
T/O-US; ASTM-D1894
Film Tensile Strength at Break, MD 120 MPa
17400 psi
ASTM-D882
Film Tensile Strength at Break, TD 260 MPa
37700 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 80 %
80 %
ASTM-D1003
Gloss 3.0 %
3.0 %
ASTM-D2457
Descriptive Properties Value Comments
Wetting Tension (Dyn) 38
ASTM-D2578
Yield (m²/kg) 76.6
Kinlead