Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 30 µm)

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Kinlead
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 30 µm).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrapping, textiles, and other packaging with a printing requirement.Information provided by Kinlead.
Physical Properties Metric English Comments
Thickness 30.0 microns
1.18 mil
± 2.5%; ASTM-252-78
Linear Mold Shrinkage 0.040 cm/cm
0.040 in/in
ASTM-D1204
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ASTM-D1204
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 160 %
160 %
ASTM-D882
Film Elongation at Break, TD 60 %
60 %
ASTM-D882
Coefficient of Friction 0.35
0.35
T/T-US; ASTM-D1894
0.40
0.40
T/O-US; ASTM-D1894
Film Tensile Strength at Break, MD 155 MPa
22500 psi
ASTM-D882
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 1.1 %
1.1 %
ASTM-D1003
Gloss 94 %
94 %
ASTM-D2457
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Wetting Tension (Dyn) 38
ASTM-D2578
Yield (m²/kg) 36.6
Kinlead
Users viewing this material also viewed the following: