Kobe Steel KS6-2-4-2 Alpha Titanium Alloy, AMS 4976, Solution treated and aged

Category Metal , Nonferrous Metal , Titanium Alloy
Manufacturer Kobe Steel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kobe Steel KS6-2-4-2 Alpha Titanium Alloy, AMS 4976, Solution treated and aged.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nominal Composition: Ti-6 Al-2 Sn-4 Zr-2 Mo Applications: Jet engine parts, engine valves.Features:Heat resistant. Information provided by Kobe Steel
Physical Properties Metric English Comments
Density 4.54 g/cc
0.164 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 896 MPa
>= 130000 psi
Tensile Strength, Yield >= 827 MPa
>= 120000 psi
0.2% proof
Elongation at Break >= 10 %
>= 10 %
Reduction of Area >= 25 %
>= 25 %
Component Elements Properties Metric English Comments
Aluminum, Al 5.5 - 6.5 %
5.5 - 6.5 %
Carbon, C <= 0.050 %
<= 0.050 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.10 %
<= 0.10 %
Molybdenum, Mo 1.8 - 2.2 %
1.8 - 2.2 %
Nitrogen, N <= 0.050 %
<= 0.050 %
Oxygen, O <= 0.15 %
<= 0.15 %
Silicon, Si 0.060 - 0.10 %
0.060 - 0.10 %
Tin, Sn 1.8 - 2.2 %
1.8 - 2.2 %
Titanium, Ti >= 84.235 %
>= 84.235 %
As Remainder
Zirconium, Zr 3.6 - 4.4 %
3.6 - 4.4 %