Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 199 - 210 °C | 390 - 410 °F | |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 199 - 210 °C | 390 - 410 °F | |
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Melt Temperature | 199 - 204 °C | 390 - 399 °F | |
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 199 - 210 °C | 390 - 410 °F | |
PolyOne Stat-Tech™ AT-10CF/000 Acetal (POM) Copolymer Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 199 - 210 °C | 390 - 410 °F | |
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 199 - 232 °C | 390 - 450 °F | |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Melt Temperature | 199 - 216 °C | 390 - 420 °F | |
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade ALATHON L5005V is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typical applicati.. |
|||
Melt Temperature | 199 - 232 °C | 390 - 450 °F | |
Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1442A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1662-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1709C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1871 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2315 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2334-R2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2349 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1351J Thermoplastic Elastomer Uses: Consumer Applications; Gaskets; Plumbing Parts; Pump Parts Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a p.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1852A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1855PV2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2434G Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Consumer Applications; Gaskets; Medical/Healthcare Applications; Membranes; Packaging; Safety Equipment; Sporting Goods; Tape; Tubing Forms: Pellets Processing Method: Fi.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2560B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2581A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2602G Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2760 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2760BR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2970 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-3017 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 232 °C | 390 - 450 °F | film extrusion |
Total PPR 8473 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8473 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The very .. |
|||
Melt Temperature | 199 - 232 °C | 390 - 450 °F | Processing |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2564A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 266 °C | 390 - 510 °F | Average value: 244 °C Grade Count:14 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |