| Category | Fluid , Solvent |
| Manufacturer | LyondellBasell |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LyondellBasell DPNP Dipropylene glycol normal propyl ether.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.922 g/cc | 0.922 g/cc | 20/20°C |
| Density | 0.923 g/cc @Temperature 20.0 °C |
0.0333 lb/in³ @Temperature 68.0 °F |
|
| Solubility in Water | 18 % | 18 % | 20°C |
| Viscosity | 4.4 cP @Temperature 25.0 °C |
4.4 cP @Temperature 77.0 °F |
|
| Molecular Weight | 176.3 g/mol | 176.3 g/mol | |
| Vapor Pressure | 0.0000667 bar @Temperature 20.0 °C |
0.0500 torr @Temperature 68.0 °F |
|
| Evaporation Loss | 1.3 % | 1.3 % | n-BuAc=100% |
| Surface Tension | 25.8 dynes/cm | 25.8 dynes/cm | 25°C |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Boiling Point | 212 °C | 414 °F | at 760 mmHg |
| Flash Point | 88.0 °C | 190 °F | Seta |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.422 @Temperature 25.0 °C |
1.422 @Temperature 77.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| CAS Number | 29911-27-1 |