Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Polyplastics Co.
Trade Name Duranex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers or other inorganic filler additives. Various grades are available, including flame-retardant, reinforced, and impact-resistant grades. DURANEX®, due to its mechanical strength, heat stability, electrical resistivity and wear and abrasion-resistance, offers great potential as a well-balanced, highly reliable material, having a wide variety of applications including electronic / electro-mechanical and automobile parts and various other functional parts. DURANEX® also assures moldability, dimensional stability, glossy surfaces and various fabrication capabilities providing higher added value.Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
ISO 1183
Filler Content 30 %
30 %
Glass fiber
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 143 MPa
20700 psi
ISO 527-1, 2
Elongation at Break 2.0 %
2.0 %
ISO 527-1, 2
Flexural Strength 224 MPa
32500 psi
ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
ISO 178
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
11.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 211 °C
412 °F
ISO 75-1, 2
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 60093
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
IEC 60093
Dielectric Strength 20.0 kV/mm
508 kV/in
IEC 60243-1
Comparative Tracking Index 250 V
250 V
IEC 60112