Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA285003 Medium Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA285003 Medium Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsPETROTHENE NA 285-003 is a medium density polyethylene resin for blown or cast film extrusion. Typical applications include overwrap film. This product exhibits good film optics and high stiffness. Regulatory StatusNA 285-003 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing NA 285-003 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.Physical PropertiesThese are typical values and not to be construed as specific product limits. Film gauge: 1.25 mils.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 6.2 g/10 min
6.2 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 500 %
500 %
ASTM D882
Film Elongation at Break, TD 600 %
600 %
ASTM D882
Dart Drop Test 60.0 g
0.132 lb
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
Film Tensile Strength at Break, TD 29.0 MPa
4200 psi
ASTM D882
1% Secant Modulus, MD 262 MPa
38000 psi
ASTM D882
1% Secant Modulus, TD 296 MPa
43000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 65 %
65 %
at 45°; ASTM D2457
Users viewing this material also viewed the following: